fig6
Figure 6. (A) Calculated κs by the Debye-Callaway model with different phonon scattering mechanisms; (B) Schematic illustration of the evolution of Ge-vacancy defects and carrier and phonon transport after high-temperature sintering[105]; (C) Structural model of a quantum gap in a Ge-Bi-Te alloy viewed along the [110]PC zone axis; the quantum gap allows carriers to pass through while strongly scattering phonons. Figure 6C is adapted from Ref.[106] under the CC BY 4.0 license; (D) Low-magnification transmission electron microscopy (TEM) images of the Ge-deficient samples sintered at 723K and 873K, respectively. Figure 6B and D is adapted from Ref.[105] under the CC BY 4.0 license; (E) Schematic diagram illustrates the phonon scattering introduced by defect engineering. Figure 6A and E is adapted from Ref.[103] with permission. Copyright © 2024 Wiley; (F) Bright-field scanning transmission electron microscopy (STEM) image of Ge0.94Pb0.05Te0.96(BiSe)0.04 sample indicating the grain size distribution; (G) STEM image showing the presence of intragrain 2D defects and the Ge at the grain boundaries; The temperature-dependent (H) lattice thermal conductivity and (I) ZT of Ge1-xPbxTe0.96(BiSe)0.04 samples. Figure 6F-I is adapted from Ref.[110] with permission. Copyright © 2025 Wiley. ZT: Dimensionless figure of merit.