fig2
Figure 2. (A) Relationship between thermoelectric parameters and carrier concentration. Figure 2A is adapted from Ref.[45] with permission. Copyright © 2016 American Chemical Society; (B) Composition-dependent carrier concentration for Ge1-x-yPbxSbyTe at room temperature. The different symbols denote samples with different Pb and Sb contents: black squares, ySb = 0 (xPb = 0-0.10); purple squares, xPb = 0.10 (ySb = 0-0.05); green triangles, xPb = 0.15 (ySb = 0-0.05); red circles, xPb = 0.20 (ySb = 0-0.05). Figure 2B is adapted from Ref.[38] with permission. Copyright © 2018 American Chemical Society; (C) Evolution of n for GeTe samples annealed at 773 and 623 K, respectively. Figure 2C is adapted from Ref.[46] with permission. Copyright © 2023 Wiley; (D) Annealing time dependence of hole density and mobility. Figure 2D is adapted from Ref.[61] under the CC BY 4.0 license. ZT: Dimensionless figure of merit.