Figure 2. Powder XRD patterns of the different CAM + LLZO:Ga mixtures obtained after co-sintering at 1,000 °C using Cu kα1/2 radiation. All intensities are normalized to the LLZO:Ga reflection (024) at ~30.8 °2θ. (M = Ni, Co, Mn).