fig7

Figure 7. (A) Schematic representation of NVPF growth. Reproduced with permission[192]. Copyright 2024, Royal Society of Chemistry; (B) Electron cloud density of associated materials. Reproduced with permission[193]. Copyright 2024, Wiley -VCH; (C) TEM image of NVPF particle; (D) Schematic representation of the effects of NaPAA and PVDF binders on the formation of CEI layers. Reproduced with permission[194]. Copyright 2024, Royal Society of Chemistry; (E) Schematic representation of the Na4C6O6 loss compensation mechanism for the cathode and anode. Reproduced with permission[195]. Copyright 2022, Royal Society of Chemistry. NVPF: